What is Wave Soldering?
Princípio de funcionamento dos sistemas de soldadura por onda
- Turbulent wave – It is quite thin but very fast. It has a very strong upward as well as sideways flow. It is capable of pushing solder in very small holes and around the leads of components. Because of this, it is unlikely that any joint area will be left unfilled, even if it is very difficult to access.
- Laminar wave – The smooth and broad wave that comes after the turbulent wave. It eliminates the excess solder, cuts down the possibility of bridging, and results in a neat and bright fillet.
Etapas do processo de soldadura por onda
Step 1: Flux Application
Step 2: Preheating
Step 3: Soldering Wave Contact
Step 4: Cooling
Optional Step: Cleaning
Wave Soldering Machine & Wave Soldering Flux
- Flux applicator – Different methods like foam, spray or wave are used to apply wave soldering flux
- Preheat zone – The temperature of the board is gradually increased by the use of infrared or convection heaters.
- Solder pot with wave nozzle – The solder pot contains molten solder, and a pump is used to create the solder wave.
- Zona de arrefecimento – The joints are solidified by the use of forced air or inert gas.
- Conveyor system – The PCB is moved through all the zones at a controlled angle and speed by the conveyor.
| Flux Type | Caraterísticas | Cleaning Required |
| Rosin-based | Good activity, leaves residues | Yes (solvent) |
| Water-soluble | High activity, corrosive residues | Yes (deionized water) |
| No-clean | Low residues, minimal activity | Não |
Selective Wave Soldering for Mixed-Technology Boards
- Protect SMDs from both thermal shock and mechanical damage
- Reduce the amount of solder and flux used
- Eliminate the need for expensive carrier pallets used for the covering of certain areas
- Perfect for low-to-medium volume manufacturing and prototyping
Wave Soldering for SMD Components
- Adhesive selection – if done properly, the correct dosed epoxy or acrylic adhesive is the thing that will hold the SMD in place during the wave without any movement.
- Component alignment – The transport direction is set by the longer axis of the SMD. It is the orientation that will result in minimal or no shadowing, and solder will get to the terminations very smoothly.
- Pad layout – Pairs of solder pads need to be spaced so as not to allow them to bridge each other. Besides the distances between pads, the shortening of the lengths of the pads is also to be considered.
- Types of components – Basic passive components like chip resistors & capacitors (0402, 0603, 0805, 1206) are suitable. Fine-pitch ICs, connectors, and BGA packages are incompatible.
- It is restricted to components having exposed terminations on the underside of the board only.
- The introduction of adhesive materials means both cost of materials and process.
- With increasing component density the possibility of solder bridging is raised.
- Not all SMDs are capable of withstanding the thermal shock of the solder wave.
Wave Soldering vs. Reflow Soldering
| Característica | Soldadura por Onda | Soldadura por Refluxo |
| Primary Use | Soldering THT (DIP) components. | Soldering Surface Mount Device (SMD) components. |
| Solder Application | Solder is applied via a dynamic wave during the process. | Solder is pre-applied as paste (a mixture of powder and flux) before component placement. |
| Princípio do Processo | The board’s underside is exposed to a wave of molten solder. | The entire board passes through a controlled, multi-zone oven where the pre-applied solder paste melts (reflows). |
| Thermal Profile | High thermal mass process; the board is heated from below by the solder itself. | A carefully managed temperature profile (preheat, soak, reflow, cooling) heats the entire assembly. |
| Typical Application | Boards with mostly THT components, or mixed technology with SMDs on top side only. | Boards with mostly or exclusively SMD components. |
| Custo | Lower for mass THT | Higher due to paste printing and ovens |
| Common Issues | Bridging, solder balls | Tombstoning, voids |
- Wave soldering is suitable for thru-hole components while reflow soldering is suitable for surface mounted components.
- For mixed technology boards, manufacturers typically do a reflow step first and follow it with wave (or selective wave) soldering for thru-hole components.
- Since only the bottom of the board in wave soldering is exposed to heat, the upper/top side components which are sensitive to heat get protection.
- Reflow soldering needs a careful temperature profile; in wave soldering the main parameters are wave height, conveyor speed, and preheating.
Wave Soldering vs Hand Soldering
| Aspeto | Soldadura por Onda | Hand Soldering |
| Velocidade | Hundreds of joints per second | One joint at a time |
| Consistency | High – machine-controlled | Operator-dependent |
| Operator skill | Minimal (setup only) | Critical for quality |
| Cost per joint | Very low (high volume) | High (labor-intensive) |
| Flexibilidade | Fixed process | Adaptable for rework, prototypes |
-
Velocidade – An entire PCB can be soldered in a wave soldering machine in seconds. If hand soldering is done on the same board, it might take minutes or even hours, according to the number of joints.
-
Consistency – The wave solder process delivers identical results across thousands of boards. Hand soldering quality varies with operator fatigue, technique, and tip condition.
-
Best use cases – Wave soldering is designed for through-hole board produção em massa. Hand soldering is still a must for prototipagem, small batches, rework, and components that do not tolerate wave soldering (e.g. heat-sensitive parts, odd-form components).
-
Custo – For volumes beyond a few hundred boards, wave soldering is the most cost-effective way by far. Hand soldering is only economically feasible for baixo volume or specialized work.
Prós e contras da soldadura por onda
- High throughput – solders hundreds or thousands of joints per board in seconds.
- Low cost per joint for mass production.
- Solder joint quality remains the same all the time.
- Fully automated, reducing labor dependency.
- Suitable for a wide range of through-hole component sizes.
- Can also solder certain SMD components (with adhesive).
- Possibility of thermal shock for delicate components or very thin boards
- Not suitable for fine-pitch SMDs or double-sided SMT boards.
- High cost of initial equipment and need for large floor space.
- Irregular board shapes need solder pallets or fixtures.
- Lead-free soldering involves higher temperature and more maintenance.
- Flux residues may require cleaning depending on flux type.
- Problems like bridging, insufficient fill, or voids will need very good process tuning.
Common Defects & Troubleshooting Tips
| Defeito | Descrição | Possible Causes | Troubleshooting Tips |
| Bridging | Solder connects two adjacent pins | – Excessive wave height – Conveyor speed too slow – Poor pad design – Insufficient flux | Reduce wave height, increase speed, check flux coverage, adjust conveyor angle |
| Insufficient fill | Solder does not fully fill the plated through-hole | – Low preheat temperature – Poor hole wetting – Conveyor speed too fast | Increase preheat, slow down conveyor, check flux activity, verify hole quality |
| Pinholes / Blowholes | Small voids or holes in solder joint | – Trapped moisture or outgassing – Contaminated board or leads – Excessive flux | Bake boards before soldering, clean boards, adjust flux amount |
| Solder balls | Small solder spheres on board surface | – Solder splashing from wave – Excess flux – High conveyor speed | Lower wave height, reduce flux, adjust speed, check flux preheating |
| Icicles | Sharp, cone-shaped solder protrusions | – Insufficient preheat – Conveyor speed too fast – Poor wave separation | Increase preheat, reduce speed, ensure proper laminar wave separation |
| No solder (skip) | Missing solder on some pins | – Warped board – Insufficient flux – Low wave height | Use board support tooling, check flux coverage, raise wave height |
Conclusão
FAQs about Wave Soldering
Faça parceria com a FS Technology e obtenha serviços profissionais de montagem de placas de circuito impresso (PCBA).
Blogues relacionados
Table of Contents Design Rule Checking in PCB Design: From Altium DRC to SMT Assembly Published on September 10, 2024 · Updated on October 22,
Table of Contents What is an Integrated Circuit (IC): Types, Working Principle & Manufacturing Process This article was originally published in Aug 2023 and last
Sumário Componentes SMD: Guia para Iniciantes em Dispositivos de Montagem em Superfície Este artigo foi originalmente publicado em novembro de 2022 e atualizado pela última vez em junho…
Sumário SMT vs SMD: Qual a diferença entre SMD e SMT? Um guia completo sobre a tecnologia de montagem em superfície (SMT) e os componentes de montagem em superfície…
Table of Contents Wire Soldering 101: How to Solder Wires to a Circuit Board Soldering wire is the fundamental skill in electronics where wire to
Índice Como melhorar a durabilidade e a longevidade dos PCBAs Os PCBs e PCBAs são amplamente utilizados em muitos dispositivos electrónicos e são essenciais para a eletrónica