Índice
Solder Paste in PCB Assembly: Selection, Printing, Defects & Expert Tips
This article was originally published in Jan 2023 and last updated on July 19, 2026.
What is Solder Paste and Why Use it?
- Low Melting Point: Given the heat sensitivity of the components, it should have a low melting point. In case the melting point is too high, there could be a possibility of the components being subjected to the maximum possible heat before completely melting.
- High Conductivity: It serves the purpose of not only making physical contact but also providing the electrical connection to enable the free flow of electrical current through the components.
- Compliant to RoHS Directive: The use of solder paste should be done such that it complies with the strict guidelines set by the Diretiva RoHS.
Solder Paste Type: Particle Size, Flux & Alloy
By Particle Size (Powder Type)
Grau de Pasta de Solda | Tamanho da partícula |
Tipo 1 | 75mm a 150mm |
Tipo 2 | 45mm a 75mm |
Tipo 3 | 25mm a 45mm |
Tipo 4 | 20mm a 38mm |
Tipo 5 | 10mm a 25mm |
Tipo 6 | 5mm a 15mm |
Tipo 7 | 2mm a 11mm |
Tipo 8 | 2mm a 8mm |
By Flux Type
- Pasta de fluxo solúvel em água: Composto por componentes orgânicos e à base de etilenoglicol. Os resíduos de fluxo solúvel em água podem ser facilmente removidos utilizando produtos de limpeza facilmente disponíveis no mercado.
- Pasta de solda não limpa: Este tipo de pasta de solda é normalmente utilizado no fabrico de fluxos não limpos. Tem um teor relativamente baixo de resíduos sólidos e de resina. A principal vantagem da utilização de um fluxo "no-clean" é a potencial poupança de custos em material de limpeza.
- Pasta de solda à base de colofónia: As pastas de soldadura deste tipo são feitas de colofónia e podem ser limpas com solventes após a soldadura.
By Alloy Composition
- SAC305 (Sn96.5/Ag3.0/Cu0.5): Industry standard for lead-free soldering applications. Provides the optimal combination of cost, thermal fatigue resistance, and wetting properties, thus suitable for all general-purpose applications such as automobiles and industrial electronics.
- Low Temperature Alloys (for example, Sn-Bi): Used for components that require low temperature or when secondary reflow is necessary, with primary solder joints remaining intact.
- High Reliability Alloys: Sometimes containing additional elements such as Nickel or Bismuth to improve drop shock and creep resistance, critical for aeroespacial e médico devices.
How to Select the Right Solder Paste for Your PCBA Project?
| Project Factor | Recommended Solder Paste Characteristics | Rationale |
| Component Density & Miniaturization | For high-density boards with 0201/01005 components and <0.4mm pitch BGAs, choose Type 4 or Type 5 powder with fine particle size. | Finer powders ensure better print release and prevent clogging in narrow apertures, reducing the risk of insufficient solder. |
| Product Reliability Requirements | For automotive, medical, or aerospace applications, opt for ROL0 (low-activity) no-clean flux combined with SAC305 or high-reliability alloys. | Low-activity flux leaves minimal ionic residues, preventing electrochemical migration. High-reliability alloys offer superior thermal cycling and shock resistance. |
| Production Volume & Mix | For high-mix, low-volume or prototype runs, Jet Printing with a fluid solder paste offers flexibility. For mass production, stencil printing with Type 4 paste is cost-effective. | Jet printing eliminates stencil costs and allows quick changeovers. Stencil printing provides high throughput for repetitive jobs. |
| Conformidade regulamentar | If your products are exported to EU or North America, ensure the solder paste is RoHS-compliant (lead-free). For medical implants, also consider biocompatible alloys. | Non-compliance can lead to legal barriers and market rejection. |
| Process Window & Equipment | Match the paste’s viscosity to your printing equipment (squeegee speed, pressure). Also, ensure your reflow oven can handle the recommended temperature profile. | Incompatible viscosity causes smearing or insufficient release. Wrong profile leads to cold joints or component damage. |
Best Practices for Solder Paste Storage and Handling
- Shelf Life: At normal temperatures (22 °C/72 °F), solder pastes usually have a storage life of between three and six months. Unrefrigerated: 25 °C (77 °F) / Refrigerated: 0°-12 °C (32 °F-55 °F).
- Avoid Heat: The performance of solder paste may be impacted by exposure to temperatures above 30 °C (85 °F). Keep solder paste away from heat sources that are hotter than 32 °C (90 °F).
- Orientation: When feasible, store solder pastes in syringes or cartridges vertically, tip down. Packages should occasionally be turned 180 degrees if they are horizontally stored.
- FIFO System: Paste must be used before the date indicated on the product-specific TDS, which is the Date of Manufacturing (DOM) on the label. On a FIFO system with the date and time of removal from storage recorded, the oldest solder paste lots should be utilized first.
Critical Handling Rules
- Do Not Use Cold: Cold usage of solder paste is not permitted. Before opening the paste package, filler material should be allowed to attain room temperature, which is 68°–77 °F (20°–25 °C). Normally, this takes between four and six hours. DO NOT HEAT THE PASTE FORCEFULLY (e.g., using a heat gun), as this causes condensation and flux separation.
- Mixing: A pasta de solda em frascos deve ser leve e bem misturada com uma ferramenta de plástico durante pelo menos um minuto após ter atingido a temperatura ambiente. As seringas e cartuchos para pasta de solda não precisam de ser misturados. Não é aconselhável utilizar equipamento automático de mistura de pasta de solda, uma vez que poderia danificar a pasta de solda.
PCB Solder Paste Printing: 3 Solder Paste Application Methods
Stencil Printing (Mass Production Standard)
Jet Printing (For Flexibility and Prototyping)
Manual Application (For Rework and Hobbyists)
- Utilizando uma seringa, aplique com precisão a pasta de solda nos pinos e, em seguida, utilize um ferro de soldar para a unir aos pinos.
- Coloque o fio de solda entre os dois pinos do componente e, em seguida, utilize um ferro de soldar para o aquecer.
Common Solder Paste Defects and How to Prevent Them
| Defeito | Visual Appearance | Primary Causes | Prevention & Corrective Actions |
| Solder Bridging | Solder connects two adjacent pads or pins, creating a short circuit. | Excessive solder paste volume; stencil apertures too large; low paste viscosity; improper squeegee pressure. | Reduce stencil thickness or aperture size; adjust printing pressure; use higher viscosity paste; ensure proper alignment. |
| Tombstoning (Manhattan Effect) | One end of a chip component lifts off the pad, standing upright. | Uneven solder paste deposition on the two pads; different thermal mass on pads; rapid heating during reflow. | Ensure uniform paste volume on both pads; optimize reflow profile (soak zone); use nitrogen atmosphere to balance wetting forces. |
| Solder Beading (Solder Balls) | Small spherical solder balls scattered around the pad or under components. | Paste slump (spreading) before reflow; excessive oxidation; fast ramp-up rate causing spattering. | Use paste with higher viscosity and anti-slump properties; control reflow profile with a gradual ramp; ensure stencil aperture design prevents paste bleeding. |
| Insufficient Solder (Open Joint) | Pad is not fully covered; component lead appears dry or lifted. | Stencil clogged; insufficient paste volume; poor stencil release; worn squeegee. | Clean stencil regularly (under-stencil wiping); increase aperture size or stencil thickness; check squeegee condition; perform SPI to catch volume variations. |
| Poor Wetting / Cold Joint | Solder does not spread properly; appears dull, grainy, or has a non-wetting surface. | Inadequate flux activity; contaminated pads/components (oxidation); reflow temperature too low or time too short. | Choose appropriate flux (ROL1/ROL2); bake PCBs prior to assembly to remove moisture; verify reflow profile with thermocouple. |
| Voids (in BGA/CSP) | X-ray reveals gas bubbles within the solder ball. | Outgassing from flux or PCB/component surface; insufficient preheat; too rapid cooling. | Optimize reflow profile with longer soak; use low-voiding flux paste; ensure components and boards are dry. |
Conclusão
FAQs about Solder Paste
Blogues relacionados
Table of Contents Medical PCBA Cost in 2026: What Really Drives the 2.5–4× Premium Over Commercial Boards Medical PCBA costs do not only depend on
Table of Contents PCBA Functional Testing (FCT): A Complete Guide to Ensuring Board Reliability Published on May 9, 2023 · Updated on November 6, 2026
Table of Contents IPC Class 2 vs Class 3: Acceptance Criteria, Cost Impact, and How to Choose IPC Class 2 and Class 3 are the
Table of Contents Ventilator PCB Assembly: ISO 13485, IPC Class 3 & FDA QMSR-Ready Manufacturing Published on June 24, 2022 · Updated on October 30,
Table of Contents Ventilator PCB Assembly: ISO 13485, IPC Class 3 & FDA QMSR-Ready Manufacturing How is air delivered steadily with the help of ventilators,
Table of Contents Automotive PCB Assembly: The Complete 2026 OEM Guide Failure of a consumer good is a warranty claim. Failure of an automotive printed
Partner with us & Start your PBCA Project