目次

Solder Paste in PCB Assembly: Selection, Printing, Defects & Expert Tips

This article was originally published in Jan 2023 and last updated on July 19, 2026.

A crucial component in electronic devices is the PCBA board, consisting of two main parts: プリント基板 と コンポーネント. The PCB supports and connects the components, which, in turn, provide the actual functionality. Initially, these two parts are separate, but through the assembly and soldering process, they are eventually combined into a unified whole.
 
In this assembly process, the use of certain key materials is necessary, and one of these is はんだペースト. This article will provide a detailed overview of the role of solder paste and a guide on how to correctly use solder paste in the PCB組立工程.
Solder Paste in SMT Assembly

What is Solder Paste and Why Use it?

One of the most reliable methods to connect two metals without melting them is soldering, and solder paste is essential for achieving this. はんだペースト is a special metal alloy composed of metal solder particles and a unique combination of flux. During the soldering process, the distinctive properties of solder paste allow it to melt and form a permanent bond, thus establishing a reliable connection between metals.
 
To ensure good performance during the soldering process, solder paste must meet several important standards:
  1. Low Melting Point: Given the heat sensitivity of the components, it should have a low melting point. In case the melting point is too high, there could be a possibility of the components being subjected to the maximum possible heat before completely melting.
  2. High Conductivity: It serves the purpose of not only making physical contact but also providing the electrical connection to enable the free flow of electrical current through the components.
  3. Compliant to RoHS Directive: The use of solder paste should be done such that it complies with the strict guidelines set by the RoHS指令.
 
In the past, approximately 40% of solder pastes in electronic manufacturing consisted of a combination of lead and tin. However, due to the environmental hazards associated with lead, and with advancements in technology and increased environmental awareness, the 電子製造 industry has gradually transitioned to lead-free processes. Consequently, lead-free solder paste has become the mainstream choice, reflecting a positive response to environmental concerns and industry focus on health and sustainability.
PCB組み立て時のソルダーペースト印刷

Solder Paste Type: Particle Size, Flux & Alloy

PCBA基板の品質を確保するためには、高品質で正しいタイプのソルダーペーストを使用することが重要です。組立プロジェクトにおいて、FSテクノロジーは様々な要求を満たすために、様々なグレードとタイプのソルダーペーストを提供しています。はんだ付けを予定している材料やニーズに応じて選択したり、はんだペースト中のはんだボールの大きさに応じて選択することができます。

By Particle Size (Powder Type)

さまざまなプロジェクトの要件を満たすために、はんだペーストは通常、異なるグレードとカテゴリに分かれています。これらの等級は、はんだボールの正確なサイズのみに基づいているわけではなく、はんだボールの約80%が特定のサイズ範囲に収まるかどうかに基づいて評価されます。以下に各種グレードとそれに対応するはんだボールサイズを示します。

ソルダーペーストのグレード

粒子径

タイプ1

75mm~150mm

タイプ2

45mm~75mm

タイプ3

25mm~45mm

タイプ4

20mm~38mm

タイプ5

10mm~25mm

タイプ6

5mm〜15mm

タイプ7

2mm~11mm

タイプ8

2mm~8mm

プロのアドバイス
For standard SMT assembly with 0603 components and 0.4mm pitch ICs, Type 4 solder paste (20-38μm) is the most versatile and widely recommended choice. For ultra-fine pitch applications like 01005 components, Type 5 or finer is required.

By Flux Type

粒子径を考慮するだけでなく、フラックスの種類によって適切なソルダーペーストを選択することも有効な選択肢です。異なるタイプの PCBフラックス は、より良いはんだ付け結果を得るため、または特定のプロセス要件を満たすために、特定のはんだペースト配合によりよく適合させることができます。ただし、すべての環境でこのタイプのフラックスを使用できるわけではなく、十分にクリーンな環境であることを確認する必要があります。
  • 水溶性フラックスペースト: 有機成分とエチレングリコールベースで構成されている。水溶性フラックスの残渣は、市販の洗浄剤で簡単に除去できる。
  • 無洗浄ソルダーペースト: このタイプのソルダーペーストは通常、無洗浄フラックスの製造に使用される。固形残留物や樹脂含有量が比較的少ない。無洗浄フラックスを使用する主な利点は、洗浄用品のコストを削減できる可能性があることです。
  • ロジン系ソルダーペースト: この種のはんだペーストはロジンから作られており、はんだ付け後に溶剤を使って洗浄することができる。

By Alloy Composition

Whereas the original passage is concerned about the size of particles, the choice of alloy is just as important. The selection of alloy will determine the melting temperature, mechanical strength, and reliability of the solder joint.
  • SAC305 (Sn96.5/Ag3.0/Cu0.5): Industry standard for lead-free soldering applications. Provides the optimal combination of cost, thermal fatigue resistance, and wetting properties, thus suitable for all general-purpose applications such as automobiles and industrial electronics.
  • Low Temperature Alloys (for example, Sn-Bi): Used for components that require low temperature or when secondary reflow is necessary, with primary solder joints remaining intact.
  • High Reliability Alloys: Sometimes containing additional elements such as Nickel or Bismuth to improve drop shock and creep resistance, critical for 航空宇宙 と メディカル devices.

How to Select the Right Solder Paste for Your PCBA Project?

The selection of an appropriate type of solder paste is not universal. In order to have a high yield rate and reliability, you need to consider your project based on the following criteria. Please use the decision guide together with the technical information above.
Project FactorRecommended Solder Paste CharacteristicsRationale
Component Density & MiniaturizationFor high-density boards with 0201/01005 components and <0.4mm pitch BGAs, choose Type 4 or Type 5 powder with fine particle size.Finer powders ensure better print release and prevent clogging in narrow apertures, reducing the risk of insufficient solder.
Product Reliability RequirementsFor automotive, medical, or aerospace applications, opt for ROL0 (low-activity) no-clean flux combined with SAC305 or high-reliability alloys.Low-activity flux leaves minimal ionic residues, preventing electrochemical migration. High-reliability alloys offer superior thermal cycling and shock resistance.
Production Volume & MixFor high-mix, low-volume or prototype runs, Jet Printing with a fluid solder paste offers flexibility. For mass production, stencil printing with Type 4 paste is cost-effective.Jet printing eliminates stencil costs and allows quick changeovers. Stencil printing provides high throughput for repetitive jobs.
規制遵守If your products are exported to EU or North America, ensure the solder paste is RoHS-compliant (lead-free). For medical implants, also consider biocompatible alloys.Non-compliance can lead to legal barriers and market rejection.
Process Window & EquipmentMatch the paste’s viscosity to your printing equipment (squeegee speed, pressure). Also, ensure your reflow oven can handle the recommended temperature profile.Incompatible viscosity causes smearing or insufficient release. Wrong profile leads to cold joints or component damage.
Recommendation from FS Technology:
In case of general electronics applications such as consumer and industrial controls, which account to about 80%, we advise the use of SAC305 Alloy in combination with Type 4 and No-clean ROL1 Flux, as it offers the most reliable solution at an affordable price. For specific needs, our engineering team is available for personalized consultation.

Best Practices for Solder Paste Storage and Handling

Solder Paste Storage in FS TECH
の温度と湿度によって異なる。 PCBA工場すぐに使用できるソルダーペーストは、製品の温度を0°~30 °C(86°F~84°F)に保つよう特別に設計されたパッケージに入れ、最低48時間保管してください。
 
ソルダーペーストは、夜間輸送またはチルド輸送でお願いします。夏期は時間短縮と高温を避けるため、なるべく夜間に輸送してください。ペーストの梱包には保冷剤が含まれている場合があり、これが溶けて届くことがあります。48時間の輸送時間を超えていない場合、これは典型的な現象であり、損傷や不適切な取り扱いの兆候ではありません。到着後、ソルダーペーストはすぐに管理された保管場所に移動する必要があります。冷蔵の使用をお勧めしますが、必ずしも必要ではありません。
 
Detailed Storage Guidelines:
  • Shelf Life: At normal temperatures (22 °C/72 °F), solder pastes usually have a storage life of between three and six months. Unrefrigerated: 25 °C (77 °F) / Refrigerated: 0°-12 °C (32 °F-55 °F).
  • Avoid Heat: The performance of solder paste may be impacted by exposure to temperatures above 30 °C (85 °F). Keep solder paste away from heat sources that are hotter than 32 °C (90 °F).
  • Orientation: When feasible, store solder pastes in syringes or cartridges vertically, tip down. Packages should occasionally be turned 180 degrees if they are horizontally stored.
  • FIFO System: Paste must be used before the date indicated on the product-specific TDS, which is the Date of Manufacturing (DOM) on the label. On a FIFO system with the date and time of removal from storage recorded, the oldest solder paste lots should be utilized first.
 

Critical Handling Rules

  • Do Not Use Cold: Cold usage of solder paste is not permitted. Before opening the paste package, filler material should be allowed to attain room temperature, which is 68°–77 °F (20°–25 °C). Normally, this takes between four and six hours. DO NOT HEAT THE PASTE FORCEFULLY (e.g., using a heat gun), as this causes condensation and flux separation.
  • Mixing: 瓶入りのはんだペーストは、常温に戻してから1分以上、プラスチック製の器具で軽くよく混ぜてください。シリンジやカートリッジは混ぜる必要はありません。また、自動混合装置を使用すると、はんだペーストに悪影響を及ぼすことがありますので、使用しないでください。

PCB Solder Paste Printing: 3 Solder Paste Application Methods

This is the most critical step in SMTアセンブリ, as over 70% of soldering defects originate from the printing process. There are three primary methods to apply solder paste onto the PCB.
solder paste printing in SMT line

Stencil Printing (Mass Production Standard)

最も一般的な方法はステンシル印刷で、これは通常ステンレス鋼製の特殊な金属グリッド構造である。メーカーはまず PCBステンシル with holes or apertures of the same size and shape as the surface mount pads in the design. To ensure accuracy, FS Technology employs laser cutting technology to process the stencil and applies a coating material on the surface to smooth the apertures and facilitate even distribution of solder paste.
 
その後、ステンシルをSMT装置内に設置し、下のPCBと位置合わせを行う。はんだペーストが均一にステンシル上に塗布され、スキージーブレードで余分なペーストをこすり落とし、開口部からPCB表面に滴下させる。全工程の所要時間は通常約15秒から45秒。
 
Post-Printing Inspection:
ソルダーペースト印刷完了後 SPI (Solder Paste Inspection) testing is conducted to assess the uniformity and quality of the solder paste, ensuring each pad receives the correct coverage in terms of height, area, and volume. Finally, the stencil is cleaned after completing a batch of PCB solder paste printing to ensure that residue from the previous printing does not impact the distribution of solder paste on the next board.
ソルダーペーストの検査

Jet Printing (For Flexibility and Prototyping)

孔版印刷は、次のような場合に有利である。 大規模PCBアセンブリしかし、ステンシルの作成にはかなりの時間がかかり、各部品のはんだペースト量を正確に制御することは困難です。そのため、ジェット印刷がますます普及しています。
 
ジェット印刷は、より液状に近いソルダーペーストを作成するために改良された配合を利用します。インクジェットプリンターは、ステンシル印刷と同じPCB設計データを使用して、基板上の各インターフェースパッドに正確な量のはんだペーストを塗布します。アプリケーションに必要なはんだ材料に応じて、プリンターははんだペーストカートリッジを簡単に切り替えて使用することができます。
 
Advantage:
ジェットプリンティング技術により、PCBアセンブラーは各インターフェイスのソルダーペースト量を正確に制御することができ、大幅な柔軟性が得られます。つまり、各ソルダーポイントのソルダーペースト量を特定の要件に基づいて調整することができます。 プロトタイプ and high-mix 少量生産.

Manual Application (For Rework and Hobbyists)

修理や趣味のプロジェクトでは、プリント基板にソルダーペーストを塗布するために印刷法を採用することは通常ありません。その代わりに、2つの一般的な手作業による方法がある:
  • 注射器を使い、はんだペーストをピンに正確に塗布し、はんだごてを使ってピンとはんだペーストを接着する。
  • はんだ線を部品の2本のピンの間に置き、はんだごてで加熱する。
 
Regardless of the method chosen, the ultimate goal is to establish a reliable connection between the PCB and the component. After manual soldering is completed, it is advisable to perform a quality check and conduct 機能テスト to ensure the reliability of the connections.
PCBステンシル印刷

Common Solder Paste Defects and How to Prevent Them

Even with proper materials and equipment, soldering defects can occur. Recognizing the root causes and implementing preventive measures is key to maintaining high yield. Below are the most frequent defects encountered in SMT assembly, along with practical solutions.
欠陥Visual AppearancePrimary CausesPrevention & Corrective Actions
Solder BridgingSolder connects two adjacent pads or pins, creating a short circuit.Excessive solder paste volume; stencil apertures too large; low paste viscosity; improper squeegee pressure.Reduce stencil thickness or aperture size; adjust printing pressure; use higher viscosity paste; ensure proper alignment.
Tombstoning (Manhattan Effect)One end of a chip component lifts off the pad, standing upright.Uneven solder paste deposition on the two pads; different thermal mass on pads; rapid heating during reflow.Ensure uniform paste volume on both pads; optimize reflow profile (soak zone); use nitrogen atmosphere to balance wetting forces.
Solder Beading (Solder Balls)Small spherical solder balls scattered around the pad or under components.Paste slump (spreading) before reflow; excessive oxidation; fast ramp-up rate causing spattering.Use paste with higher viscosity and anti-slump properties; control reflow profile with a gradual ramp; ensure stencil aperture design prevents paste bleeding.
Insufficient Solder (Open Joint)Pad is not fully covered; component lead appears dry or lifted.Stencil clogged; insufficient paste volume; poor stencil release; worn squeegee.Clean stencil regularly (under-stencil wiping); increase aperture size or stencil thickness; check squeegee condition; perform SPI to catch volume variations.
Poor Wetting / Cold JointSolder does not spread properly; appears dull, grainy, or has a non-wetting surface.Inadequate flux activity; contaminated pads/components (oxidation); reflow temperature too low or time too short.Choose appropriate flux (ROL1/ROL2); bake PCBs prior to assembly to remove moisture; verify reflow profile with thermocouple.
Voids (in BGA/CSP)X-ray reveals gas bubbles within the solder ball.Outgassing from flux or PCB/component surface; insufficient preheat; too rapid cooling.Optimize reflow profile with longer soak; use low-voiding flux paste; ensure components and boards are dry.
FS Technology’s Quality Assurance:
We employ SPI inspection after printing and AOI(自動光学検査) plus レントゲン after reflow to detect and eliminate these defects at every stage, ensuring your PCBA meets IPC Class 2 or Class 3 standards.

結論

Solder paste is the lifeblood of modern SMT assembly. From selecting the correct alloy and particle size (Type 3, 4, or 5) to rigorous storage protocols and precise printing processes, every step impacts the final quality of your PCBA.
 
で FSテクノロジー, we combine state-of-the-art equipment (including advanced SPI and jet printing systems) with strict process control to ensure your boards are assembled with the highest reliability. Whether you need high-volume production or ラピッドプロトタイピング, our engineering team is ready to assist you in selecting the optimal solder paste for your specific application.
 

FAQs about Solder Paste

The difference lies in the powder particle size. Type 3 ranges from 25-45μm and is suitable for standard components and larger pitch ICs. Type 4 ranges from 20-38μm and is required for finer pitch components like 0201 and 0.4mm pitch BGAs, providing better print release and reduced solder balling.
Yes, but the temperature must be strictly controlled between 0°C and 12°C (32°F-55°F). Do not freeze the paste. Also, ensure the container is sealed tightly to prevent moisture absorption.
This is called “conditioning” . It allows the entire container of paste to reach room temperature evenly. If opened cold, moisture from the air will condense on the cold paste, leading to solder spatter and voids during reflow.
Typically, this is due to low humidity in the environment, prolonged exposure to air (draft), or a stencil temperature that is too high. It is recommended to keep the production environment at 22-28°C and 40-60% relative humidity, and to return unused paste to the jar if printing pauses for more than 30 minutes.
Use a solder paste formulated with low-voiding flux, optimize the reflow profile with a longer soak zone to allow outgassing, and ensure both the PCB and BGA components are properly baked to remove moisture prior to assembly.

関連ブログ

Partner with us & Start your PBCA Project