Table des matières
Solder Paste in PCB Assembly: Selection, Printing, Defects & Expert Tips
This article was originally published in Jan 2023 and last updated on July 19, 2026.
What is Solder Paste and Why Use it?
- Low Melting Point: Given the heat sensitivity of the components, it should have a low melting point. In case the melting point is too high, there could be a possibility of the components being subjected to the maximum possible heat before completely melting.
- High Conductivity: It serves the purpose of not only making physical contact but also providing the electrical connection to enable the free flow of electrical current through the components.
- Compliant to RoHS Directive: The use of solder paste should be done such that it complies with the strict guidelines set by the Directive RoHS.
Solder Paste Type: Particle Size, Flux & Alloy
By Particle Size (Powder Type)
Qualité de la pâte à braser | Taille de la particule |
Type 1 | 75mm à 150mm |
Type 2 | 45mm à 75mm |
Type 3 | 25mm à 45mm |
Type 4 | 20mm à 38mm |
Type 5 | 10mm à 25mm |
Type 6 | 5mm à 15mm |
Type 7 | 2mm à 11mm |
Type 8 | 2mm à 8mm |
By Flux Type
- Pâte de flux soluble dans l'eau : Composé de composants organiques et d'une base d'éthylène glycol. Les résidus de flux solubles dans l'eau peuvent être facilement éliminés à l'aide de produits de nettoyage disponibles sur le marché.
- Pâte à braser sans nettoyage : Ce type de pâte à braser est généralement utilisé dans la fabrication de flux sans nettoyage. Elle contient relativement peu de résidus solides et de résine. Le principal avantage de l'utilisation d'un flux sans nettoyage est l'économie potentielle sur les produits de nettoyage.
- Pâte à braser à base de colophane : Les pâtes à souder de ce type sont fabriquées à partir de colophane et peuvent être nettoyées à l'aide de solvants après la soudure.
By Alloy Composition
- SAC305 (Sn96.5/Ag3.0/Cu0.5): Industry standard for lead-free soldering applications. Provides the optimal combination of cost, thermal fatigue resistance, and wetting properties, thus suitable for all general-purpose applications such as automobiles and industrial electronics.
- Low Temperature Alloys (for example, Sn-Bi): Used for components that require low temperature or when secondary reflow is necessary, with primary solder joints remaining intact.
- High Reliability Alloys: Sometimes containing additional elements such as Nickel or Bismuth to improve drop shock and creep resistance, critical for aérospatiale et médical devices.
How to Select the Right Solder Paste for Your PCBA Project?
| Project Factor | Recommended Solder Paste Characteristics | Rationale |
| Component Density & Miniaturization | For high-density boards with 0201/01005 components and <0.4mm pitch BGAs, choose Type 4 or Type 5 powder with fine particle size. | Finer powders ensure better print release and prevent clogging in narrow apertures, reducing the risk of insufficient solder. |
| Product Reliability Requirements | For automotive, medical, or aerospace applications, opt for ROL0 (low-activity) no-clean flux combined with SAC305 or high-reliability alloys. | Low-activity flux leaves minimal ionic residues, preventing electrochemical migration. High-reliability alloys offer superior thermal cycling and shock resistance. |
| Production Volume & Mix | For high-mix, low-volume or prototype runs, Jet Printing with a fluid solder paste offers flexibility. For mass production, stencil printing with Type 4 paste is cost-effective. | Jet printing eliminates stencil costs and allows quick changeovers. Stencil printing provides high throughput for repetitive jobs. |
| Conformité réglementaire | If your products are exported to EU or North America, ensure the solder paste is RoHS-compliant (lead-free). For medical implants, also consider biocompatible alloys. | Non-compliance can lead to legal barriers and market rejection. |
| Process Window & Equipment | Match the paste’s viscosity to your printing equipment (squeegee speed, pressure). Also, ensure your reflow oven can handle the recommended temperature profile. | Incompatible viscosity causes smearing or insufficient release. Wrong profile leads to cold joints or component damage. |
Best Practices for Solder Paste Storage and Handling
- Shelf Life: At normal temperatures (22 °C/72 °F), solder pastes usually have a storage life of between three and six months. Unrefrigerated: 25 °C (77 °F) / Refrigerated: 0°-12 °C (32 °F-55 °F).
- Avoid Heat: The performance of solder paste may be impacted by exposure to temperatures above 30 °C (85 °F). Keep solder paste away from heat sources that are hotter than 32 °C (90 °F).
- Orientation: When feasible, store solder pastes in syringes or cartridges vertically, tip down. Packages should occasionally be turned 180 degrees if they are horizontally stored.
- FIFO System: Paste must be used before the date indicated on the product-specific TDS, which is the Date of Manufacturing (DOM) on the label. On a FIFO system with the date and time of removal from storage recorded, the oldest solder paste lots should be utilized first.
Critical Handling Rules
- Do Not Use Cold: Cold usage of solder paste is not permitted. Before opening the paste package, filler material should be allowed to attain room temperature, which is 68°–77 °F (20°–25 °C). Normally, this takes between four and six hours. DO NOT HEAT THE PASTE FORCEFULLY (e.g., using a heat gun), as this causes condensation and flux separation.
- Mixing: La pâte à souder en pot doit être légèrement et soigneusement mélangée avec un outil en plastique pendant au moins une minute après avoir atteint la température ambiante. Les seringues et les cartouches de pâte à braser n'ont pas besoin d'être mélangées. Il n'est pas conseillé d'utiliser un équipement automatisé pour mélanger la pâte à braser, car cela pourrait endommager la pâte à braser.
PCB Solder Paste Printing: 3 Solder Paste Application Methods
Stencil Printing (Mass Production Standard)
Jet Printing (For Flexibility and Prototyping)
Manual Application (For Rework and Hobbyists)
- À l'aide d'une seringue, appliquez précisément la pâte à souder sur les broches, puis utilisez un fer à souder pour la faire adhérer aux broches.
- Placez le fil de soudure entre les deux broches du composant, puis utilisez un fer à souder pour le chauffer.
Common Solder Paste Defects and How to Prevent Them
| Défaut | Visual Appearance | Primary Causes | Prevention & Corrective Actions |
| Solder Bridging | Solder connects two adjacent pads or pins, creating a short circuit. | Excessive solder paste volume; stencil apertures too large; low paste viscosity; improper squeegee pressure. | Reduce stencil thickness or aperture size; adjust printing pressure; use higher viscosity paste; ensure proper alignment. |
| Tombstoning (Manhattan Effect) | One end of a chip component lifts off the pad, standing upright. | Uneven solder paste deposition on the two pads; different thermal mass on pads; rapid heating during reflow. | Ensure uniform paste volume on both pads; optimize reflow profile (soak zone); use nitrogen atmosphere to balance wetting forces. |
| Solder Beading (Solder Balls) | Small spherical solder balls scattered around the pad or under components. | Paste slump (spreading) before reflow; excessive oxidation; fast ramp-up rate causing spattering. | Use paste with higher viscosity and anti-slump properties; control reflow profile with a gradual ramp; ensure stencil aperture design prevents paste bleeding. |
| Insufficient Solder (Open Joint) | Pad is not fully covered; component lead appears dry or lifted. | Stencil clogged; insufficient paste volume; poor stencil release; worn squeegee. | Clean stencil regularly (under-stencil wiping); increase aperture size or stencil thickness; check squeegee condition; perform SPI to catch volume variations. |
| Poor Wetting / Cold Joint | Solder does not spread properly; appears dull, grainy, or has a non-wetting surface. | Inadequate flux activity; contaminated pads/components (oxidation); reflow temperature too low or time too short. | Choose appropriate flux (ROL1/ROL2); bake PCBs prior to assembly to remove moisture; verify reflow profile with thermocouple. |
| Voids (in BGA/CSP) | X-ray reveals gas bubbles within the solder ball. | Outgassing from flux or PCB/component surface; insufficient preheat; too rapid cooling. | Optimize reflow profile with longer soak; use low-voiding flux paste; ensure components and boards are dry. |
Conclusion
FAQs about Solder Paste
Blogs associés
Table of Contents Medical PCBA Cost in 2026: What Really Drives the 2.5–4× Premium Over Commercial Boards Medical PCBA costs do not only depend on
Table of Contents PCBA Functional Testing (FCT): A Complete Guide to Ensuring Board Reliability Published on May 9, 2023 · Updated on November 6, 2026
Table of Contents IPC Class 2 vs Class 3: Acceptance Criteria, Cost Impact, and How to Choose IPC Class 2 and Class 3 are the
Table of Contents Ventilator PCB Assembly: ISO 13485, IPC Class 3 & FDA QMSR-Ready Manufacturing Published on June 24, 2022 · Updated on October 30,
Table of Contents Ventilator PCB Assembly: ISO 13485, IPC Class 3 & FDA QMSR-Ready Manufacturing How is air delivered steadily with the help of ventilators,
Table of Contents Automotive PCB Assembly: The Complete 2026 OEM Guide Failure of a consumer good is a warranty claim. Failure of an automotive printed
Partner with us & Start your PBCA Project