Inhaltsverzeichnis

Solder Paste in PCB Assembly: Selection, Printing, Defects & Expert Tips

This article was originally published in Jan 2023 and last updated on July 19, 2026.

A crucial component in electronic devices is the PCBA board, consisting of two main parts: PCB und Komponenten. The PCB supports and connects the components, which, in turn, provide the actual functionality. Initially, these two parts are separate, but through the assembly and soldering process, they are eventually combined into a unified whole.
 
In this assembly process, the use of certain key materials is necessary, and one of these is Lotpaste. This article will provide a detailed overview of the role of solder paste and a guide on how to correctly use solder paste in the PCB Montageprozess.
Solder Paste in SMT Assembly

What is Solder Paste and Why Use it?

One of the most reliable methods to connect two metals without melting them is soldering, and solder paste is essential for achieving this. Lötpaste is a special metal alloy composed of metal solder particles and a unique combination of flux. During the soldering process, the distinctive properties of solder paste allow it to melt and form a permanent bond, thus establishing a reliable connection between metals.
 
To ensure good performance during the soldering process, solder paste must meet several important standards:
  1. Low Melting Point: Given the heat sensitivity of the components, it should have a low melting point. In case the melting point is too high, there could be a possibility of the components being subjected to the maximum possible heat before completely melting.
  2. High Conductivity: It serves the purpose of not only making physical contact but also providing the electrical connection to enable the free flow of electrical current through the components.
  3. Compliant to RoHS Directive: The use of solder paste should be done such that it complies with the strict guidelines set by the RoHS-Richtlinie.
 
In the past, approximately 40% of solder pastes in electronic manufacturing consisted of a combination of lead and tin. However, due to the environmental hazards associated with lead, and with advancements in technology and increased environmental awareness, the elektronische Fertigung industry has gradually transitioned to lead-free processes. Consequently, lead-free solder paste has become the mainstream choice, reflecting a positive response to environmental concerns and industry focus on health and sustainability.
Lotpastendruck bei der PCB-Bestückung

Solder Paste Type: Particle Size, Flux & Alloy

Die Verwendung von hochwertiger und richtiger Lötpaste ist ein entscheidender Schritt zur Gewährleistung der Qualität von PCBA-Platinen. Für Bestückungsprojekte bietet FS Technology verschiedene Qualitäten und Typen von Lötpasten an, die unterschiedlichen Anforderungen gerecht werden. Sie können je nach den für das Löten vorgesehenen Materialien und den Anforderungen wählen oder nach der Größe der Lotkugeln in der Lötpaste auswählen.

By Particle Size (Powder Type)

Um den Anforderungen verschiedener Projekte gerecht zu werden, werden Lötpasten in der Regel in verschiedene Qualitäten und Kategorien eingeteilt. Diese Klassen basieren nicht nur auf der genauen Größe der Lötkugeln, sondern werden auf der Grundlage von etwa 80% der Lötkugeln bewertet, die in einen bestimmten Größenbereich fallen. Hier sind die verschiedenen Klassen und die entsprechenden Lotkugelgrößen.

Qualität der Lötpaste

Größe des Partikels

Typ 1

75mm bis 150mm

Typ 2

45mm bis 75mm

Typ 3

25mm bis 45mm

Typ 4

20mm bis 38mm

Typ 5

10mm bis 25mm

Typ 6

5mm bis 15mm

Typ 7

2mm bis 11mm

Typ 8

2mm bis 8mm

Profi-Tipp:
For standard SMT assembly with 0603 components and 0.4mm pitch ICs, Type 4 solder paste (20-38μm) is the most versatile and widely recommended choice. For ultra-fine pitch applications like 01005 components, Type 5 or finer is required.

By Flux Type

Neben der Berücksichtigung der Partikelgröße ist auch die Wahl der geeigneten Lotpaste auf der Grundlage der Art des Flussmittels eine sinnvolle Option. Verschiedene Arten von PCB-Flussmittel kann besser auf bestimmte Lotpastenformulierungen abgestimmt werden, um bessere Lötergebnisse zu erzielen oder bestimmte Prozessanforderungen zu erfüllen. Allerdings erlauben nicht alle Umgebungen die Verwendung dieser Art von Flussmittel, und es muss sichergestellt werden, dass die Umgebung sauber genug ist.
  • Wasserlösliche Flussmittelpaste: Besteht aus organischen Bestandteilen und Ethylenglykol-Basis. Rückstände von wasserlöslichem Flussmittel lassen sich mit handelsüblichen Reinigungsmitteln leicht entfernen.
  • No-Clean Lötpaste: Diese Art von Lotpaste wird typischerweise bei der Herstellung von No-Clean-Flussmitteln verwendet. Sie hat relativ wenig feste Rückstände und einen geringen Harzanteil. Der Hauptvorteil der Verwendung eines No-Clean-Flussmittels sind die möglichen Kosteneinsparungen bei den Reinigungsmitteln.
  • Lötpaste auf Kolophoniumbasis: Solche Lötpasten werden aus Kolophonium hergestellt und können nach dem Löten mit Lösungsmitteln gereinigt werden.

By Alloy Composition

Whereas the original passage is concerned about the size of particles, the choice of alloy is just as important. The selection of alloy will determine the melting temperature, mechanical strength, and reliability of the solder joint.
  • SAC305 (Sn96.5/Ag3.0/Cu0.5): Industry standard for lead-free soldering applications. Provides the optimal combination of cost, thermal fatigue resistance, and wetting properties, thus suitable for all general-purpose applications such as automobiles and industrial electronics.
  • Low Temperature Alloys (for example, Sn-Bi): Used for components that require low temperature or when secondary reflow is necessary, with primary solder joints remaining intact.
  • High Reliability Alloys: Sometimes containing additional elements such as Nickel or Bismuth to improve drop shock and creep resistance, critical for Luft- und Raumfahrt und medizinisch devices.

How to Select the Right Solder Paste for Your PCBA Project?

The selection of an appropriate type of solder paste is not universal. In order to have a high yield rate and reliability, you need to consider your project based on the following criteria. Please use the decision guide together with the technical information above.
Project FactorRecommended Solder Paste CharacteristicsRationale
Component Density & MiniaturizationFor high-density boards with 0201/01005 components and <0.4mm pitch BGAs, choose Type 4 or Type 5 powder with fine particle size.Finer powders ensure better print release and prevent clogging in narrow apertures, reducing the risk of insufficient solder.
Product Reliability RequirementsFor automotive, medical, or aerospace applications, opt for ROL0 (low-activity) no-clean flux combined with SAC305 or high-reliability alloys.Low-activity flux leaves minimal ionic residues, preventing electrochemical migration. High-reliability alloys offer superior thermal cycling and shock resistance.
Production Volume & MixFor high-mix, low-volume or prototype runs, Jet Printing with a fluid solder paste offers flexibility. For mass production, stencil printing with Type 4 paste is cost-effective.Jet printing eliminates stencil costs and allows quick changeovers. Stencil printing provides high throughput for repetitive jobs.
Einhaltung gesetzlicher VorschriftenIf your products are exported to EU or North America, ensure the solder paste is RoHS-compliant (lead-free). For medical implants, also consider biocompatible alloys.Non-compliance can lead to legal barriers and market rejection.
Process Window & EquipmentMatch the paste’s viscosity to your printing equipment (squeegee speed, pressure). Also, ensure your reflow oven can handle the recommended temperature profile.Incompatible viscosity causes smearing or insufficient release. Wrong profile leads to cold joints or component damage.
Recommendation from FS Technology:
In case of general electronics applications such as consumer and industrial controls, which account to about 80%, we advise the use of SAC305 Alloy in combination with Type 4 and No-clean ROL1 Flux, as it offers the most reliable solution at an affordable price. For specific needs, our engineering team is available for personalized consultation.

Best Practices for Solder Paste Storage and Handling

Solder Paste Storage in FS TECH
Je nach Temperatur und Feuchtigkeit des PCBA-FabrikBewahren Sie diese gebrauchsfertigen Lötpasten in einer speziellen Verpackung auf, die die Temperatur des Produkts mindestens 48 Stunden lang zwischen 0° und 30 °C (86 °F und 84 °F) hält.
 
Lötpaste sollte über Nacht oder durch gekühlten Transport geliefert werden. Im Sommer sollte der Transport so weit wie möglich nachts erfolgen, um die Zeit zu verkürzen und hohe Temperaturen zu vermeiden. Die Pastenverpackung kann Kühlakkus enthalten, die schmelzend ankommen. Wenn die 48-Stunden-Reisezeit nicht überschritten wird, ist dies typisch und kein Zeichen für eine Beschädigung oder unsachgemäße Behandlung. Nach der Ankunft muss die Lötpaste sofort in ein kontrolliertes Lager gebracht werden. Eine Kühlung wird empfohlen, ist aber nicht immer erforderlich.
 
Detailed Storage Guidelines:
  • Shelf Life: At normal temperatures (22 °C/72 °F), solder pastes usually have a storage life of between three and six months. Unrefrigerated: 25 °C (77 °F) / Refrigerated: 0°-12 °C (32 °F-55 °F).
  • Avoid Heat: The performance of solder paste may be impacted by exposure to temperatures above 30 °C (85 °F). Keep solder paste away from heat sources that are hotter than 32 °C (90 °F).
  • Orientation: When feasible, store solder pastes in syringes or cartridges vertically, tip down. Packages should occasionally be turned 180 degrees if they are horizontally stored.
  • FIFO System: Paste must be used before the date indicated on the product-specific TDS, which is the Date of Manufacturing (DOM) on the label. On a FIFO system with the date and time of removal from storage recorded, the oldest solder paste lots should be utilized first.
 

Critical Handling Rules

  • Do Not Use Cold: Cold usage of solder paste is not permitted. Before opening the paste package, filler material should be allowed to attain room temperature, which is 68°–77 °F (20°–25 °C). Normally, this takes between four and six hours. DO NOT HEAT THE PASTE FORCEFULLY (e.g., using a heat gun), as this causes condensation and flux separation.
  • Mixing: Die Lotpaste in Gläsern sollte, nachdem sie Raumtemperatur erreicht hat, mindestens eine Minute lang mit einem Kunststoffwerkzeug leicht und gründlich gemischt werden. Spritzen und Kartuschen für Lotpaste müssen nicht gemischt werden. Von der Verwendung automatischer Mischgeräte für Lotpaste ist abzuraten, da sie die Lotpaste beschädigen könnten.

PCB Solder Paste Printing: 3 Solder Paste Application Methods

This is the most critical step in SMT-Bestückung, as over 70% of soldering defects originate from the printing process. There are three primary methods to apply solder paste onto the PCB.
solder paste printing in SMT line

Stencil Printing (Mass Production Standard)

Das gängigste Verfahren ist der Schablonendruck, bei dem es sich um eine spezielle Metallgitterstruktur handelt, die in der Regel aus rostfreiem Stahl besteht. Die Hersteller erstellen zunächst eine PCB-Schablone with holes or apertures of the same size and shape as the surface mount pads in the design. To ensure accuracy, FS Technology employs laser cutting technology to process the stencil and applies a coating material on the surface to smooth the apertures and facilitate even distribution of solder paste.
 
Die Schablone wird dann in eine SMT-Vorrichtung eingesetzt und an der darunter liegenden Leiterplatte ausgerichtet. Die Lötpaste wird gleichmäßig auf die Schablone aufgetragen und mit einem Rakelmesser wird die überschüssige Paste abgekratzt, so dass sie durch die Öffnungen auf die Leiterplattenoberfläche tropft. Der gesamte Vorgang dauert in der Regel etwa 15 bis 45 Sekunden.
 
Post-Printing Inspection:
Nachdem der Lotpastendruck abgeschlossen ist, SPI (Lötpasteninspektion) testing is conducted to assess the uniformity and quality of the solder paste, ensuring each pad receives the correct coverage in terms of height, area, and volume. Finally, the stencil is cleaned after completing a batch of PCB solder paste printing to ensure that residue from the previous printing does not impact the distribution of solder paste on the next board.
Inspektion von Lötpaste

Jet Printing (For Flexibility and Prototyping)

Der Schablonendruck ist zwar vorteilhaft für PCB-Bestückung im großen StilDie Herstellung der Schablone ist sehr zeitaufwendig und die genaue Kontrolle der Lotpastenmenge für jedes Bauteil ist eine Herausforderung. Daher wird das Jet Printing immer beliebter.
 
Beim Jet Printing wird eine modifizierte Formel verwendet, um eine flüssigere Lotpaste zu erzeugen. Tintenstrahldrucker verwenden dieselben Leiterplattendesigndaten wie beim Schablonendruck und tragen eine präzise Menge an Lotpaste auf jedes Schnittstellenpad auf der Leiterplatte auf. Je nach dem für die Anwendung benötigten Lotmaterial kann der Drucker einfach zwischen Lotpastenkartuschen wechseln, aus denen winzige Tropfen Lotpaste herausgespritzt werden.
 
Advantage:
Mit der Jet Printing Technologie können Leiterplattenbestücker die Menge der Lötpaste für jede Schnittstelle genau steuern, was ihnen eine erhebliche Flexibilität bietet. Das bedeutet, dass die Lotpastenmenge für jede Lötstelle je nach den spezifischen Anforderungen angepasst werden kann. Prototypen and high-mix Kleinserienproduktion.

Manual Application (For Rework and Hobbyists)

Bei Reparatur- oder Bastelprojekten wird die Druckmethode in der Regel nicht verwendet, um Lotpaste auf Leiterplatten aufzutragen. Stattdessen gibt es zwei gängige manuelle Methoden:
  • Tragen Sie mit einer Spritze präzise Lötpaste auf die Stifte auf und verwenden Sie dann einen Lötkolben, um sie mit den Stiften zu verbinden.
  • Legen Sie Lötdraht zwischen die beiden Stifte des Bauteils und verwenden Sie einen Lötkolben, um ihn zu erhitzen.
 
Regardless of the method chosen, the ultimate goal is to establish a reliable connection between the PCB and the component. After manual soldering is completed, it is advisable to perform a quality check and conduct Funktionstests to ensure the reliability of the connections.
PCB Schablonendruck

Common Solder Paste Defects and How to Prevent Them

Even with proper materials and equipment, soldering defects can occur. Recognizing the root causes and implementing preventive measures is key to maintaining high yield. Below are the most frequent defects encountered in SMT assembly, along with practical solutions.
DefektVisual AppearancePrimary CausesPrevention & Corrective Actions
Solder BridgingSolder connects two adjacent pads or pins, creating a short circuit.Excessive solder paste volume; stencil apertures too large; low paste viscosity; improper squeegee pressure.Reduce stencil thickness or aperture size; adjust printing pressure; use higher viscosity paste; ensure proper alignment.
Tombstoning (Manhattan Effect)One end of a chip component lifts off the pad, standing upright.Uneven solder paste deposition on the two pads; different thermal mass on pads; rapid heating during reflow.Ensure uniform paste volume on both pads; optimize reflow profile (soak zone); use nitrogen atmosphere to balance wetting forces.
Solder Beading (Solder Balls)Small spherical solder balls scattered around the pad or under components.Paste slump (spreading) before reflow; excessive oxidation; fast ramp-up rate causing spattering.Use paste with higher viscosity and anti-slump properties; control reflow profile with a gradual ramp; ensure stencil aperture design prevents paste bleeding.
Insufficient Solder (Open Joint)Pad is not fully covered; component lead appears dry or lifted.Stencil clogged; insufficient paste volume; poor stencil release; worn squeegee.Clean stencil regularly (under-stencil wiping); increase aperture size or stencil thickness; check squeegee condition; perform SPI to catch volume variations.
Poor Wetting / Cold JointSolder does not spread properly; appears dull, grainy, or has a non-wetting surface.Inadequate flux activity; contaminated pads/components (oxidation); reflow temperature too low or time too short.Choose appropriate flux (ROL1/ROL2); bake PCBs prior to assembly to remove moisture; verify reflow profile with thermocouple.
Voids (in BGA/CSP)X-ray reveals gas bubbles within the solder ball.Outgassing from flux or PCB/component surface; insufficient preheat; too rapid cooling.Optimize reflow profile with longer soak; use low-voiding flux paste; ensure components and boards are dry.
FS Technology’s Quality Assurance:
We employ SPI inspection after printing and AOI (Automatisierte optische Inspektion) plus Röntgenstrahlen after reflow to detect and eliminate these defects at every stage, ensuring your PCBA meets IPC Class 2 or Class 3 standards.

Fazit

Solder paste is the lifeblood of modern SMT assembly. From selecting the correct alloy and particle size (Type 3, 4, or 5) to rigorous storage protocols and precise printing processes, every step impacts the final quality of your PCBA.
 
Unter FS Technologie, we combine state-of-the-art equipment (including advanced SPI and jet printing systems) with strict process control to ensure your boards are assembled with the highest reliability. Whether you need high-volume production or schnelle Prototypenerstellung, our engineering team is ready to assist you in selecting the optimal solder paste for your specific application.
 

FAQs about Solder Paste

The difference lies in the powder particle size. Type 3 ranges from 25-45μm and is suitable for standard components and larger pitch ICs. Type 4 ranges from 20-38μm and is required for finer pitch components like 0201 and 0.4mm pitch BGAs, providing better print release and reduced solder balling.
Yes, but the temperature must be strictly controlled between 0°C and 12°C (32°F-55°F). Do not freeze the paste. Also, ensure the container is sealed tightly to prevent moisture absorption.
This is called “conditioning” . It allows the entire container of paste to reach room temperature evenly. If opened cold, moisture from the air will condense on the cold paste, leading to solder spatter and voids during reflow.
Typically, this is due to low humidity in the environment, prolonged exposure to air (draft), or a stencil temperature that is too high. It is recommended to keep the production environment at 22-28°C and 40-60% relative humidity, and to return unused paste to the jar if printing pauses for more than 30 minutes.
Use a solder paste formulated with low-voiding flux, optimize the reflow profile with a longer soak zone to allow outgassing, and ensure both the PCB and BGA components are properly baked to remove moisture prior to assembly.

Verwandte Blogs

Partner with us & Start your PBCA Project